The results of the investigations of the transformation of impurity defects in natural diamonds of various habits at the stage of high-temperature annealing at P = 6 GPa and T = 2200°C are presented. The studies conducted allowed us to ascertain that the transformations of Aand B-defects in diamonds of octahedral and cubic habits follow general regularities. This fact shows that most of the diamonds of cubic habit with low degree of aggregation of nitrogen centers were not really annealed over a long-term interval. Unlike octahedral diamonds, those of cubic habit are characterized by a pronounced increase in the peak of H-containing defects (3107 cm–1) after annealing.

Язык оригиналаанглийский
Страницы (с-по)32-37
Число страниц6
ЖурналDoklady Earth Sciences
Том466
Номер выпуска1
DOI
СостояниеОпубликовано - 1 янв 2016

Fingerprint Подробные сведения о темах исследования «The transformation features of impurity defects in natural diamonds of various habits under high P–T conditions». Вместе они формируют уникальный семантический отпечаток (fingerprint).

  • Цитировать